Three series of tests were conducted on specimens with lap lengths varying from 20 to 85 bar diameters. The results indicate that increasing the length of a lap splice beyond 45 bar diameters was an inefficient way to increase the strength of...

bond bond strength Civil Engineering coupon datacenterhub deformed bar development length lap splice reinforced concrete splice lenght structural concrete structural engineering